Foorno faakiyuum ah oo aluminium ah oo PJ-VAB ah
OO AY KU JIRAAN:
Dahaarka aagga kulul ee birta aan lahayn iyo walxaha kuleylka Nichrome;
Aagagga kuleylka ee dhinacyo badan leh si loo xakameeyo heerkulka saxda ah;
Nidaamka bamgareynta faakuumka ee weyn ee loogu talagalay inuu wax ka qabto qarxinta magnesium inta lagu jiro habka daminta (faakuumka oo liita = tayada daminta oo liidata);
dabinada uumiga ee shaandheeyaha cabirka faakuumka;
Naqshadeynta wareegga xakamaynta ee isku-dhafka saamiga badan (PID) si loogu habeeyo cabbirro iyo miisaanno kala duwan oo qaybo ah;
Gaashaan si looga hortago uruurinta magnesium ee giraanta O-ring ee albaabka iyo giraanta poppet-ka ee waalka ugu weyn;
Albaab laba jibbaaran si loo fududeeyo dayactirka;
Qaab-dhismeed koronto oo gaar ah si looga fogaado suurtagalnimada qaansada wareegga gaaban;
Iyada oo la adeegsanayo saxanka ururiyaha magnesium si looga hortago in magnesium ku ururto meelaha sida foornada korontada ku shaqeysa iyo qalabka kuleylka lagu shubo - meelaha ay adkaan karto in la nadiifiyo;
Iyada oo leh dabin qaboojin gaar ah oo loogu talagalay ilaalinta bamka faafinta;
Qeexitaanka ugu muhiimsan
| Koodhka moodeelka | Cabbirka aagga shaqada mm | Awoodda culayska kg | |||
| dhererka | ballaca | dhererka | |||
| PJ-VAB | 5510 | 500 | 500 | 1000 | 500 |
| PJ-VAB | 9920 | 900 | 900 | 2000 | 1200 |
| PJ-VAB | 1225 | 1200 | 1200 | 2500 | 2000 |
| PJ-VAB | 1530 | 1500 | 1500 | 3000 | 3500 |
| PJ-VAB | 2250 | 2200 | 2200 | 5000 | 4800 |
|
Heerkulka ugu badan ee shaqada:700℃; Isku mid ahaanshaha heerkulka:≤±3℃; Faaruqinta ugu dambeysa:6.7*10-4Pa; Heerka kor u kaca cadaadiska:≤0.2Pa/saacaddii;
| |||||
Fiiro gaar ah: Cabbirka iyo qeexitaannada la habeeyey ayaa la heli karaa